An electrical steel RFQ gets a usable quote only when it fixes twelve things: grade and standard, thickness, width, delivery form, loss test point, coating, coil size, edge and burr, rolling direction, mechanical limits, certificate, and commercial terms. Leave one out and the supplier fills the gap with an assumption, and two quotes for “the same steel” stop being comparable. This guide lists the twelve items, what to write for each, the mistakes that most often produce a wrong quote, and a template you can paste into an email.

We’re Wuxi Zhongxin Special Steel (ZHX Steel). We quote CRNGO steel coil and grain-oriented coil, slit strip and sheet every week, and most of the follow-up questions we send back are about the items below.
| # | Spec | What to write | What goes wrong if it is missing |
|---|---|---|---|
| 1 | Grade and standard | One designation plus its standard, e.g. M250-35A (EN 10106) | “Silicon steel” or a bare “M4” is read differently by each supplier |
| 2 | Thickness and tolerance | Nominal thickness and the tolerance class or limit | Quotes mix nominal and tolerance-stretched material |
| 3 | Width and tolerance | Nominal width and tolerance | Slitting cost and trim are priced differently |
| 4 | Delivery form | Master coil, slit strip or cut sheet | Coil price compared against sheet price |
| 5 | Loss test point | Induction, frequency and standard, e.g. 1.5 T, 50 Hz | Loss values quoted at different conditions |
| 6 | Coating | Class, chemistry and minimum insulation value | Coating priced and tested to different levels |
| 7 | Coil ID, OD, weight | Inner diameter, maximum outer diameter, maximum coil mass | Coils that do not fit the uncoiler |
| 8 | Edge, burr, camber | Mill or slit edge, burr height limit, camber limit | Slit quality assumed, not agreed |
| 9 | Rolling direction | Which dimension runs along rolling (sheet and cut parts) | Cut parts with the wrong grain direction |
| 10 | Mechanical limits | Minimum yield, hardness range or bends, if they matter | Typical values treated as guarantees |
| 11 | Certificate | EN 10204 type and the test results to report | Certificate lacks the figures you need |
| 12 | Commercial terms | Quantity, packing, Incoterm, port, delivery date | Prices that differ only in what they include |
Material Specs: Items 1 to 4
1. Grade and standard. Name one grade in one standard. EN 10106 and IEC 60404-8-4 cover non-oriented strip and sheet, and EN 10107 and IEC 60404-8-7 cover grain-oriented. The same steel carries different names in GB, JIS and ASTM, and the digits are not comparable across systems because loss is quoted per kilogram in one and per pound in another. Our grade equivalents guide maps the systems. If you are matching an existing part, give the old designation as well, so the supplier can confirm the equivalent rather than guess it.
2. Thickness and tolerance. Give the nominal thickness and say which tolerance applies. A thickness range or an unstated tolerance lets a supplier quote at the thin end of the permitted band. Thickness also fixes the weight per square metre, which matters for settlement.
3. Width and tolerance. State the nominal width and the allowed deviation. For several widths, list each with its own quantity.
4. Delivery form. Say whether you want master coil, slit strip or cut sheet. Each is priced differently, and a coil quote cannot be compared with a sheet quote. If you need slit strip from a wider coil, say so, because trim and edge allowances change the quote. How to choose between grades is a separate decision, covered in our guide on how to choose electrical steel.
Magnetic and Coating Specs: Items 5 and 6
5. Loss test point. The number in a grade name is a maximum loss at a stated condition. For non-oriented grades that is normally 1.5 T at 50 Hz; for grain-oriented it is 1.7 T. ASTM grades quote watts per pound at 60 Hz. Write the induction, the frequency and the standard, for example “maximum 2.50 W/kg at 1.5 T, 50 Hz”. If your design runs at 400 Hz, the standard does not guarantee loss there, so ask for typical curves as well and say they are for information. Also say that the quote must be for prime material. Secondary (non-prime) coil is sold with different guarantees, and an unusually low price can mean that is what is being quoted; our guide to prime vs secondary CRGO explains how to tell.
6. Coating. Name the class (C-3, C-5 and so on), whether it must be chrome-free, and the minimum insulation value with its unit and test method. A class name alone does not fix a number. Our guide to interlaminar resistance explains the Franklin test and what to write. State whether the value must hold after stress relief annealing if your laminations will be annealed.

Coil, Edge and Direction: Items 7 to 9
7. Coil ID, OD and weight. EN 10106’s ordering clause covers details such as the coil inner diameter (for example 508 or 610 mm), the maximum coil mass and the inspection document. Give the inner diameter that fits your uncoiler, the maximum outer diameter and the maximum mass per coil, as a per-coil limit and not only a total tonnage. State whether weights are theoretical, net or gross; the arithmetic is in our guide to electrical steel density and weight.
8. Edge, burr and camber. Say whether you want mill edge or slit edge, and write a maximum burr height and a camber limit with the measurement method. Burr matters because it can bridge the insulation between laminations and speeds die wear. Slitting limits and how to measure camber are in our guide to slitting tolerances. If a burr direction matters for your press, state which side the burr should face.
9. Rolling direction. For cut sheet, state which dimension must run along the rolling direction. For grain-oriented steel this is not optional: the low loss applies only along rolling. For non-oriented steel it matters less, but still note it for punched parts. Stamping requirements for the cut parts are a separate topic.
Mechanical Limits and Paperwork: Items 10 and 11
10. Mechanical limits. EN 10106 guarantees a minimum number of bends for each grade but no yield strength, tensile strength or hardness. Mill catalogues print typical values, not guarantees. If your part depends on a minimum yield strength, a hardness range or a bend count, write it into the RFQ with the test method and direction. The grade-by-grade numbers are in our guide to electrical steel mechanical properties.
11. Certificate. Name the EN 10204 certificate type and list the results that must appear on it: loss at the stated test point, induction, thickness, stacking factor and any insulation or mechanical values you specified. If you want a third-party witness, say so. What each type covers is explained in our article on EN 10204 3.1 and 3.2 certificates.

Commercial Terms: Item 12
12. Quantity, packing, Incoterm and delivery. State total quantity and the split by grade and size, the packing basis, the Incoterm with a named port or place, and the date you need the steel. Two prices are only comparable on the same Incoterm. Our guide to Incoterms for electrical steel shows who pays for what under each term.
For what to expect on quantity and timing, see our lead times and MOQ article.
Mistakes That Produce a Wrong Quote
| Mistake | Why the quote is wrong | Fix |
|---|---|---|
| Grade given as “M4” or “silicon steel” only | Each supplier picks its own interpretation | Give grade, standard and thickness |
| Prime not stated | A low quote may be for secondary coil | Write that the quote is for prime material |
| Loss quoted without test point | A value at 1.5 T is not a value at 1.7 T | Write induction, frequency and standard |
| Coil and sheet quotes compared directly | Price bases differ | State the delivery form |
| No coil ID or maximum mass | Coil may not fit the line | Give ID, OD and per-coil limit |
| Slit edge assumed | Burr and camber limits differ by supplier | Write the limits and method |
| Typical strength read as guaranteed | Mill data is not a guarantee | Write the minimum into the RFQ |
| “Certificate included” | Required results are missing | List the results and EN 10204 type |
| Prices on different Incoterms | One quote includes freight, one does not | Fix the Incoterm and port |
RFQ Template
Copy this into an email and fill in each line.
- Grade and standard: (for example M250-35A, EN 10106), prime material
- Thickness and tolerance:
- Width and tolerance (list each width and quantity):
- Delivery form: master coil / slit strip / cut sheet
- Loss test point: (induction, frequency, standard)
- Coating: (class, chrome-free yes or no, minimum insulation value and test method)
- Coil ID, maximum OD, maximum mass per coil, weight basis:
- Edge: mill / slit; maximum burr height; camber limit:
- Rolling direction (cut parts):
- Mechanical limits, if any: (minimum yield, hardness, bends, with test method)
- Certificate: (EN 10204 type, results to report, third-party witness yes or no)
- Quantity, packing, Incoterm and port, required date:
If you cannot fill every line, send what you have plus the application, and we will say which items still need to be fixed before we quote. We supply non-oriented and grain-oriented electrical steel in coil, slit strip and sheet. Coil orders typically start at about 5 tonnes with delivery in about 15 days, and smaller lots can be cut from coil. Sheet orders typically start at about 500 kg; if you need less, tell us and we’ll do our best to meet the request. Samples typically cost USD 200 including freight, refunded when you place a production order.
FAQ
What should an electrical steel RFQ include?
At minimum: grade and standard, thickness and width with tolerances, delivery form, the loss test point, coating and insulation value, coil inner diameter and maximum mass, edge and burr limits, certificate type, quantity, Incoterm and delivery date. Add rolling direction for cut parts and mechanical limits if the part depends on strength or hardness.
Why do two electrical steel quotes for the same grade differ so much?
Usually because the quotes do not describe the same product. Differences in thickness tolerance, delivery form, coating level, edge condition, certificate scope, packing and Incoterm all change the price. Compare quotes only after confirming that each one covers the same twelve items, and ask the supplier to state any assumption it made.
Do I need to state the loss test conditions in an RFQ?
Yes. Core loss is guaranteed only at the condition in the standard, for example 1.5 T and 50 Hz for non-oriented grades or 1.7 T for grain-oriented. A figure at another induction or frequency is not comparable. If your machine runs at a higher frequency, ask for typical loss curves and mark them as information, not a guarantee.
Which certificate should I ask for?
Ask for an EN 10204 3.1 certificate for most orders, and list the results you need printed on it, such as loss, induction, thickness and any insulation or mechanical values. Choose 3.2 only if you need an independent inspector or third party to witness the tests, and say who that party is.
Can I send an RFQ if I don’t know the exact grade?
Yes. Send the application, operating frequency, efficiency or loss target, thickness range and quantity, and we will propose a grade and confirm the items still open before quoting. It is faster to give the old designation if you are replacing an existing material, because the equivalent can then be checked directly.
Ready to send your RFQ? Contact us with the filled template and we’ll confirm the matching grade and open items before quoting.